- Product Details
Keywords
- cationic dispersion rosin
- papermaking sizing agent
- cationic rosin size
Quick Details
- ProName: Cationic dispersion rosin sizing agent...
- CasNo: 8050-09-7
- Molecular Formula: C19H29COOH
- Appearance: white milky emulsion
- Application: Papermaking sizing agent
- DeliveryTime: 10 days
- PackAge: 200kg PE drum or 1000kg IBC tank
- Port: QINGDAO
- ProductionCapacity: 1000 Metric Ton/Month
- Purity: 35%
- Storage: Store it in dry, ventilated and shady ...
- LimitNum: 1 Metric Ton
Superiority
Cationic dispersion rosin's sizing rate of dispersed rosin gum is 4 times that of ordinary rosin gum and 2 times of strengthened rosin gum, and it can improve the quality of paper, reduce the amount of rosin gum, reduce the amount of aluminum sulfate and whitening agent, etc., performance Very superior, it is a replacement product of saponified rosin gum.
Details
Cationic Dispersed Rosin Size
1,The technical indicators :
Appearance: milky white liquid
Solid content: 35% ± 1
Ionicity: cationic
Particle diameter: 0.2 ~ 0.7 μm
Viscosity: ≤ 25cps (25 °C)
P H value: 3-4
Disperstiveness : easily dispersed in cold water
2.Functions:
The cationic rosin sizing agent has positive charge itself, so it can stay with the paper pulp, declining the demand of Al2(SO4)3. And it can be used when the PH is 4.5~6.5, with CaCO3 as the padding. By using our cation rosin sizing agent, can not only reduce the usage and get strong paper but also can reduce the water pollution and the corrosion of equipment. Even in summer, it can use as usual.
3.Application method:
It can be used directly or diluted by 3-5 times. We suggest that you add it continuously with metric-pump before the add point is above Add-pump or the add amount is 0.3-1.5% of Absolutely-dry-fibre after Pressure-riddle. Al2(SO4)3 can also be put into at the same place or mixture-box, paper machine pool. Sizing PH should be 4.66.5 and the white waters PH under the net should be 5-6.5.
4.Packaging:
Plastic barrel for 200kg and 1000kg.
5.Storage:
It should be avoided to meet dense alkali. We shall put it in dry, ventilated and shady and cool place, and prevent it from insolation and be freezing.